Influence of thickness and translucency of lithium disilicate ceramic on degree of conversion of resinous materials
2020
Background In this study was assessed the degree of conversion (DC) of amine-free resin cements light cured through lithium disilicate-reinforced ceramics at different thicknesses and translucency. Material and Methods Specimens were divided into 21 groups (n = 5) according to luting agent used: Variolink Esthetic LC (Light shade), RelyX Ultimate (A1 shade), and Filtek Z350 XT Flow (A1 shade); the ceramic translucency: low (LT) and high (HT); and the ceramic thickness: no ceramic (control), 0.5 mm, 1 mm, and 2 mm. A Teflon mold with (5 x 5 x 0.5 mm) was used to standardize the cement and over it the ceramic block from each group was placed. Set was cured using a polywave LED light (1200 mW/…
Clinical Behavior of Ceramic, Hybrid and Composite Onlays. A Systematic Review and Meta-Analysis
2020
A systematic review and meta-analysis was performed to analyze the survival of onlay restorations in the posterior region, their clinical behavior according to the material used (ceramic reinforced with lithium disilicate, conventional feldspathic ceramic or reinforced with leucite; hybrid materials and composite), possible complications, and the factors influencing restoration success. The systematic review was based on the preferred reporting items for systematic reviews and meta-analyses (PRISMA) statement, without publication date or language restrictions. An electronic search was made in the PubMed, Scopus, Embase, and Cochrane databases. After discarding duplicate publications and stu…
The impact of restorative material and ceramic thickness on CAD\CAM endocrowns
2019
Made available in DSpace on 2020-12-12T02:39:33Z (GMT). No. of bitstreams: 0 Previous issue date: 2019-01-01 Background: Endocrown restorations as a conservative approach to restore endodontically treated teeth still need an in vitro investigation under fatigue at different materials. This study evaluated the effect of restorative material and restoration thickness on the maximum fracture load of endocrowns subjected to cyclic loading. Material and Methods: Sixty (60) third molar teeth received an endocrown preparation with three different heights of remaining dental tissue (1.5, 3.0 or 4.5 mm). A leucite-based ceramic (LEU) and a lithium disilicate (LD) based ceramic were selected to manuf…
Shear bond strength of debonded ceramic restorations re-cemented by means of a cleaning and retreatment protocol
2019
Background As there is no standard method for re-cementing debonded partial ceramic restorations, the aim of this study was to evaluate the use of a non-invasive thermal protocol for cleaning and retreatment, and to study its influence on shear bond strength. Material and methods Twenty ceramic samples (IPS e.max CAD®) were bonded to composite cement cylinders and underwent a shear bond strength test (G1, n=20). A second group was created (G2, n=20), representing debonded restorations. To simulate debonding, the samples were artificially contaminated with composite cement. After debonding, these underwent a thermal protocol to remove remaining adhesive. After rebonding to the composite ceme…
Fracture Resistance of New Metal-Free Materials Used for CAD-CAM Fabrication of Partial Posterior Restorations
2020
Background and Objectives: To evaluate in vitro the fracture resistance and fracture type of computer-aided design and computer-aided manufacturing (CAD-CAM) materials. Materials and Methods: Discs were fabricated (10 ×
Bond strength of lithium disilicate after cleaning methods of the remaining hydrofluoric acid
2020
Background Complex implant treatments have steadily increased within implant prosthodontics. Based on the lower implant mobility, implant impressions need high accuracy in the model transfer to receive a high passive fit within the final prosthodontic restoration. To analyze the accurate 3-dimensional (3D) inter-implant-positions, a reference point is indispensable. However, there is no reference in the patients mouth, so the aim of the present study was to develop a new method based on a custom-made-measuring-aid (CMA) to assess the inter implant dimensions (InID) in patients. Material and Methods Initially an implant master model (IMM/patient equivalent) was digitized by computed tomograp…